We are looking for eilat stone from Israel.  If anyone knows of
a source, we'd appreciate the 

Hi Joanie,

I use Eilat stone a lot. I am holding in Bangkok a stock of a
few hundreds Kilos of rough material. Let me know what are you
looking for, maybe I can be of help. Please Email me directly.

Regards
Hanuman