Rainbow Calsilica - natural or manmade?

Toxicity of Rainbow Calsilica

I have the same question about “rainbow calsilica” or “Duronite” as
I think we should call it. I wonder about the presence of pigments
such as the cadmiums which can be troublesome.

I just found a site on the web which references the composition of
topcoat automotive paints. Among the pigments used are the lead
chromates (yellow, oranges, etc.) and iron oxides. If you’re
cutting/cabbing any of the "newly found like Detroitite,
calsilica, or whatever, watch out for the inhalation of these
pigments, or transfer through the skin.

Brian Corll
Brian Corll, Inc. (BCI)
1002 East Simpson Street
Mechanicsburg, PA 17055