Hi!

I was wondering, regarding quality stamping earrings, do you stamp one earring in the pair? or both earrings in the pair?

curious, as to most common best practise.

Julie

Stamp the pair. Over time, many of us lose one earring.

The troublesome task is stamping posts and ear wires, when they are made of gold or non-allergenic metal and the bulk of the earring is made of something else.