PMC paper

Friends I just received my first PMC paper. I have used the other
forms extensively, but this new stuff came with no documentation. Come
to think about it, they didn’t even say anything about the best firing
procedure! I emailed Tim McCreight and he sent me a few useful hints,
but I wonder whether any of you kind folks have learned anything
useful about this material. Thanks!

Noel

Sorry guys to post twice in such short time. I went to the web and
found the following site www.art-clay.com and they had this
about the PMC+.

cenigrade        ferniheit      minutes
900                 1650           10
850                  1550           20
800                   1470           30

hope this helps you. Karen ---- again