Hello, I have recently started experimenting with plique a jour
enameling using fine silver and Thompson’s Lead Free enamels. I have
had some success but I would like to find out more about the
technique. I have found very little on the web or at
Amazon.com. Any tips or book recommendations would be appreciated.
Thanks

WK Dunn, Try http://plique-a-jour.net/ Richard McMullen is a great
guy. Email him and I expect he will respond to you. I’ve spoken with
him about plique for an upcoming article I wrote for BENCH magazine
on laser welding a plique-a-jour piece.

Best regards,
Bob Staley
B.Staley, Goldsmiths
Precision Laser Welding