I am in need of a caster who works with heat treatable platinum. Any
would be appreciated.

Keith
keith chapman jeweler
@keith


#2

Kieth, I’m not exactly sure what you mean by ‘heat treatable’, but
I’ve had some platinum castings done for me at Stylecast 716 856 7618.


#3

Quality casting in NYC casts Hoover and Strong heat-treatable
platinum. Imperial from Canada has a sales office in Providence - I
believe they do job casting in their heat treatable platinum. Tom
Kruskal