Anyone know of the best pickle for alpaka/nickel silver? Skaylex
(sodium bisulphate dry safety pickle) leaves a coppery residue and
hydrochloric acid works well but rusts everything in my workshop.

Griffith Chemical Company makes a pickle similar to Sparex that is
used exclusively for nickle silver.

Iris Stuecklen