What is Sparex. <<

Sparex is a granular dry acid compound (sodium bisulphate) sold
in the US It’s mixed with water (2 1/2 lbs to 7 pints) & used as
a pickle. The results aree better if you heat the mixture to
about 125 F.

Dave