@wldlzrd1 there is only one Giacomo, and he is a member here.
I wonder if the perforated ceramic soldering board works on the same principal as his heavy wire grate?
~
The Omega clip is more comfortable than the old earclips that hurt after wearing for awhile. But how is that pressure controlled on the Omega clip? Furthermore, does the pressure need to be tweaked for specific customers?
@Alec in McCreight’s book, are you referring to the Tension Spring Catch which is on the Spring Clasps page in the Mechanisms section?
Here’s a thread about them: 18K omega clips