Ney Vulcan 550 - help

I lost my manual for this… I’ve figured everything out except how
to link programs together.

Each program has three temperature steps. So, in order to do a four
temperature burnout cycle (300F, 700F, 1350F, then casting temp), you
need to “link” programs.

I cannot for the life of me figure out how to do this.

Does anyone out there know?

Thanks,

  • darcy

Darcy you may call me at 620.792.3980 and I will walk you through
the procedure. It would be easier this way. 10 - 5 Robert Benham

Hi Darcy,

First let me say we are an Authorized Ney Repair Center so we can get
a new manual to you. As for linking your programs:

First need to enter both program 1 and 2 in. Then to link them press
program 1, press start, then press program 2, then press enter.

If I can help with anything else please let me know.

Thanks,

Ken Kotoski
MPG Repair