loved steves class…have taken two now and time is never
enough…I would have loved to see the tea pot… I made a small
bowl and it is still lovely… But then we also made hugh billets
3x3 and used the forge with special coal and etc. and also the
class was two weeks long… That helps…and another time regular
kilns… This all with Gene pjanowski and Marvin Jensen…
Wonderful teachers… But I liked Steves class because I could
use a small kiln and I could do all the work myself and also it
was the right size for jewelery… But don’t you love the
material… I just made a green gold ring with palladin and it is
georgus… Yeh!!!


#2

Calgang

You can see the teapot at
http://mokume-gane.com/Pages/Photos/Teapot.html

Doyou have any pictures of mokume objects that you are making?