Lori, If you are melting a lot of silver DO NOT POUR INTO AN ALUMINUM
PAN. The aluminum will melt and you will end wup witha big mess.
Melted silver poured into water will form many very interesting
shapes. Most silversmiths use the scrap for casting. The scrap can
also be exchanged for new silver. Good Luck Lee