Hi. I was wondering if anyone knows of any methods for mass
finishing stainless steel jewelry components to a high polish finish.
I feel like I’m spending most of my time these days hand-polishing
stainless pieces instead of fabricating or assembling, and I’d love
to find a way to streamline that part of the process.

Any specific suggestions would be greatly appreciated. Thanks.

Electro polishing. i have an aquaintance with a metal fabricating
company, this is what he does, the stuff comes back looking like
polished chrome plating