Hello Orchidians:
I went through the archives and came across the threads regarding
electroplating. With the price of metals shooting up (namely gold) I
would like to be able to target my mid-audience a bit better. I have
a few designs that I would like to offer in vermeil (preferably 20KT)
but feel the bill to outsource would be too great to recoup. So I
guess I am asking for Orchidian feelings on a) the Rio electroplating
system, ease of use, ability to do the job, etc.
Feel free to respond to me at @Kennedi_Milan1 if you want to
respond off-line.
Thanks!