When making jump rings, thread your saw blade through the coil to cut
the jump rings apart, and saw from the inside out. This makes sawing
the coil easier as your blade tends to slid when starting to cut from
the outside of the coil.

Brad Simon CMBJ

3 Likes

Thank you! This is a fabulous tip. I’ve been sawing them on a wooden dowel and getting awkward angles. This is much better.