Making Devcon B conforming dies

I took Susan Kingsley’s Hydraulic Die forming workshop fourteen
years ago and just got around to buying the Devcon B I need to make
some conforming dies. I hope I have enough material for more then
one die. Would anybody know the formula for mixing Devcon B Plastic
steel for figuring the specific amounts of resin and hardener for a