Back to Ganoksin | FAQ | Contact

Making 950 Platinum Ruthenium Alloy video

Now playing: Making 950 Platinum Ruthenium Alloy
2.31 min streaming video clip

Filmed at Kraftwerks from PM West, Robert Lumabao demonstrates how
one refiner makes beautiful and reliable platinum casting grain. By
utilizing hydrogen, a spectacular light show of molten platinum is
carefully blended with pure ruthenium.

Ganoksin now offers a video peek into the virtual world. Suppliers,
refiners, jewelers, and educators will contribute incredible
demonstrations on topics including casting, alloying, bench tricks,
and more. We’ll be adding new videos to our Library, so please stay
tuned!

Enjoy
Hanuman