got a facebook post from Fretz about a Magician’s ring, very cool
hammer, the “trick” with this ring is that if made properly is that
on viewing at the right angle it is a lemniscate, aka infinity symbol.
As seen on the no. one tarot card, the Magician. This ring has been
worn so there are some scratches on it. It fell out of my stock onto
my wife’s finger LOL. The hallmark is the flying unicorn for
Argentium.

I made a round ring and then bent it in a Pepe metal bender then re-
annealed and bent in a soft jawed vice. The Argentium is a 4 by 2 mm
oval wire from A & E metals Australia.

all the best
Richard