I’ve alloyed 9%Au, 7%Pt, and 84%Ag. I liked the properties so far.
Color, workability, hopefully tarnish resistance. Problem is, After
fabing a ring with crown and small bezels, the finishing is showing
what I would call firescale when I view with my optivisors. No Cu in
this so??? Anyone help me?


#2

Maybe the alloy didn’t mix. Can you post a picture to the group? CIA

[Edit]