I need a 12mm scalloped edge round probably synthetic stone in red…
a little on the orange side. I cracked a customer’s stone and I know
I’m gonna have a heck of a time replacing it. There are eight
scallops. If anyone has any ideas or can cut one please contact me at
offline.

Thanks,
Mary


#2

Hi Mary, To find a matching color stone to replace the cracked one
in a suite is not easy, especially when you have no idea what kind of
stone it is.To find the exact match, it’s better to bring the broken
one and go to a gem dealer. And if you can find the matching one, to
recut a new one is not difficult.

Hope this help,-
Tom