Hi, To everyone looking for lime sulfur spray, I just found some at
the local Agway here in Littleton, MA. It’s a Bonide product, simply
labeled “Lime Sulfur Spray”, active ingredient calcium polysulfide
30%. It costs $10 for 32 oz. This was much easier to find than I
thought it would be! MaryLou