Ketchup is mostly made from tomatoes and vinegar, so it’s a little
acidic. Google tells me its pH is 3.8-3.9 or so.
I’ve never tried it on silver before, but when I was a kid I
remember putting old copper pennies in ketchup overnight and having
them be pink and fresh in the morning. It’s basically a weak pickle
solution.
Willis Hance