One way to remove jump rings from an oval or other odd-shaped mandrel
is to wrap the mandrel with paper before winding the wire, and then
burn the paper off before removing the jump rings. – M’lou Brubaker,
Jeweler Goodland, MN http://www.craftswomen.com