Inlay wax recipe

Inlay wax is what folks use that you can get more detail with snd isnt stringy when heated? I wanna try it but its stupid exprndive so ive gathered paraffin and a beeswax mix that may be used but im hoping someone here has a recipe or suggestions!! Thankyou!

This is the inlay wax that I’m familiar with. It’s a low temp wax. It’s not super expensive and is available at most jewelry tool companies. Or are you talking about something else?

Jeff

1 Like

Ive never used it just read it was good for detail and doesnt get stringy, thank you!!

1 Like