I would like to know what the industry standard is for a gold tie
tack stem. Gauge and length, please.

Thanks!
Tracy
tracyjohnsonjewelry.com

This is what I see and use, 1/2 inch length, 1.10mm diameter (see
Stuller #57). Shorter if a lapel pin.