Identifying night stars stones

Hi…

I have a question. I have some stones and I want to know what they
are, history, anything anyone knows? They are called: "night stars"
sun sitara which appears to connect them to sun stone also called sun
sitara?

I know very little about stones. I think these are some form of
drusy (sp?) stone, meaning they have small crystals on or inside
them. These have small reflections (appearing like tiny crystals)
under the surface of the stone.

They are very beautiful, and I have some, but am not sure what they
are. Any and all help would be appreciated. I’ve tried looking this
up on the internet, but mostly come upon either contradictory
or a bunch of auctions…yet no answers. Please help? :slight_smile:

Thank you,
Kim

Hi Kim,

The results of a google search indicate that sun sitara is another
name for goldstone. Goldstone is glass.

Donna