Back to Ganoksin | FAQ | Contact

Hydrolic press

Hi All, My uncle made me a hydrolic press by modifying the plans in
Susan Kingsley’s book. I works great and cost me all of $125.00 in
materials! I use sheet acrylic for my dyes that I get from the local
glass shop. As far as repetitive shapes go, I have the Rio press
system, it works well, however I find I don’t use it much anymore. I
use the saw table that came with it for cutting my sheet acrylic for
the press so I’m assured of getting a straight up and down cut. Hope
this helps, and Happy Thanksgiving! Lisa Wow, has the weather been
beautiful in Oregon!