Hello
Is there any advantage to apply resin using a air compressor
connected seryingue dispense? thks by advance for every received
answers
daniel
Hello
Is there any advantage to apply resin using a air compressor
connected seryingue dispense? thks by advance for every received
answers
daniel
danielle, first you may want to let us know what the resin is for
and what type it is specifically, then some of use here may be able
to help you better.
I have used a vacuum (under a bell jar) when pulling resin into the
natural fractures in gemstone rough. It stabilizes the rough enough
to cut it without it falling apart.
But I don’t know what you mean by a “seryingue dispense”
Nanz Aalund
www.nanzaalund.com
I think they mean a solder paste dispenser, I have seen them used
for resin, for putting small quantities into cells for resin brooches
and the like. Cheap on E-bay from the far east.
regards,
Tim Blades