No it will not solve your 2 problems. It will take just as long if not longer than your current process and it will do the same thing to your chain. The process is, ultrasonic, steam, electoclean, rinse in distilled water, allow to air dry, electroplate, three rinses in distilled water, allow to air dry then bake in oven. The solutions are messy and sticky. BUT the process allows me to do multiple colors on the same piece by masking, plating, baking then stripping the mask and doing a second color.