Hi there I have made a hollow bangle by hammering a piece of plate around
a metal rod then pulling it through the drawplate to make chenier(tubing).
To bend it fill the tube with melted wax this stops it kinking or crushing
when bending. You need to make about 1-1.5 inches more than you need. This
is not labour efficient but great fun. Allthe best Gerald.