I like to use the plastic coated paper clips for hanging in the
ultrasonic and the pickle . Works great and is easily bent into
shapes.they come in different sizes and colors.very inexpensive . Also,
they can be threaded through difficult to hold pieces of jewelry to
give a firm grip when polishing.

Peace be with you all…
Charlie Vartanian
All That Glitters
Little Ferry, NJ

Charlie mentioned using plastic coated paper clips to dangle jewelry
from to hang in the ultrasonic etc. What I use is similar and even
finer gauge. My son was throwing out some plastic coated copper wire
that he had used for some electronics project. Some pieces are
double or twin wires and I just peel them apart and use them. I
really find this stuff useful.