Back to Ganoksin | FAQ | Contact

Gold fill tarnishing

I’m having some problems with some of my gold-fill chains darkening,
somebought from Rio, some that I made. 14K, 14/20 – is that
redundant? Anybody have any suggestions for cleaning and why it’s
turning? Should Ibe using different pickle? (I use Rio Pickle)

Thanks, Pegi