Would fusion welding work for repairing metal frame glasses? About
how much does a unit cost?

Scott, You can use the A>B> I> tack 3 cost 3400.00 and the only thing
I believe it has a hard time on is titanium. Andy "The Tool Guy"
Kroungold Sales- Tools Supplies Specialist Phone 337-262-7700 ext.
94194 Fax 800-444-4741 e-mail @Andy_Kroungold

I had purchased an ABI tac III machine at the New York Manufactures
show, it was delivered in a very timely manner. After three weeks of
working with it, I found that it is very limited in what it can do.
Two of us in my shop played and worked with it using silver, gold,
and platinum every day for a few hours, we were on the phone with the
manufactures and tried their suggestions, the machine DID NOT perform
as represented, we were very unhappy and sent it back. My suggestion
is call the company and ask to for a firm that purchased on and is
happy, call and talk with them.

Jon D.