Fixed vs variable speed magnetic tumblers

In the process of setting up my studio and I am looking at a magnetic
finishing system in the Rio catalog. One has a fixed speed and one
has a variable speed. Why I would need varied speeds and will it make
a difference (other then paying $100 more)? Any insight to this will
be appreciated