Ferric Nitrate Mixing Instructions

Linda, I spent about 30 minutes searching for this information
because I am avoiding doing some loathsome accounting tasks. Lucky
you. I like to use Google when searching the WWW: www.google.com.

First though, here’s an Orchid posting by Karen Christians, who has
extensive etching experience:

I don’t know if Karen starts with ferric nitrate crystals, however.
Perhaps Karen is reading and will clarify.

The next link points to an entry on a MEMS message board; I have no
idea what MEMS is. But, the writer suggests 10 grams or less “per
liter”. Per liter of what he doesn’t say, I assume they mean per
liter of water.
http://mail.mems-exchange.org/pipermail/mems-talk/1999-May/003884.html

And here’s a link to a table that lists metals and etchants:
http://www.elume.com/youaskedforit.html

If you understand what Baume is, then it probably gives a recipe.
Or, you can probably find out if you continue searching. I’ve
procrastinated long enough!

Christine in Littleton, Massachusetts, USA, which has been
transformed into a winter wonderland by a late winter dusting of snow.