Back to Ganoksin | FAQ | Contact

[Favorite tips] Setting Square Stones

When channel setting square stones, a tapered square hole must be
cut to accommodate the pavilion of the stone. One method to
accomplish this is by first using a hart bur held perpendicular to
the mounting to cut the four-corners. Then, use a small wheel bur
to remove the metal between the corner cuts.Brad Simon CMBJ