When setting marquise stones, bend the side prongs over the stone
first. Then when tight bend the tip prongs or V-Tips over the points
of the stone to protect them from chipping. When setting pear shaped
stones, first bend the point prong or V-Tip. Then place the stone
into the crown, and push the remaining prongs over the stone to
secure it.

Brad Simon CMBJ