Here is a bench tip for all you polishers.Having trouble
polishing inside of tubes or small holes and the like? Take that
split mandrel you have been using for sand paper and cut a piece
of suede or ultrasuede or I suppose even a piece of cotton cloth
and fit it into the split mandrel. You have a long thin round
buff that you can vary the diameter of by the size of the piece
of cloth. I use it for polishing exterior curved surfaces as
well. Be sure and wear that dust mask. Frank