Instead of applying oil to my ingot mold I use “Spray n Cook”
(or any other household non - stick spray). Ingots are easily
extracted plus no smoke and no smell. Carefull not to spray in
the direction of your torch flame otherwise you will be holding
a flame thrower in one hand and your torch in the other.

Cheers

Alan Rathbone