Back to Ganoksin | FAQ | Contact

[Favorite tips] Carry tools


#1

Hi, For those who have to carry their tools each days like
students. You can carry your saw blades in empty Bic ball pen.
Take the refill out with the writing point and keep the two ends.
This is just the goods size for saw blades. Vincent Guy Audette


#2

Another carrying container to be used for ones saw blades is an
empty “paint ball” container ( the kind people use in their
-paint ball war games ). <-> Ruben <->