Does anyone know if lead free Thompson P-3 underglaze will work with older Thompson leaded enamels?

If not what underglaze do I need and where can I buy it?

Thanks!

Lolirw30, Yes it works perfectly.

1 Like

Thank you Karlette!

Tips and Tricks: Un leaded goes Un der

2 Likes