Follow up on the Ditto Clear experience. I made a mistake on the
proportions of catalyst versus material so probably why some of
it was tacky. Still, I made the second mold tonite and it took 2
hours to do. You have to vacuum the stuff and even though the
very confusing tech sheet says vacuuming beyond a certain point
isn’t necessery, I had to vacuum way beyond that time because
there were nice little bubbles clinging to my model. This stuff
is a pain in the butt and darn expensive too, probably will only
be using it for special purposes…Dave