I am searching for someone to stamp out, cut out or etch out multiple
units of some jewelry related shapes in 18K yellow gold and also in
mild steel sheet stock of approximately 0.50mm thickness. Can you
direct me to a good source for this service? These would be very
small production runs of approximately 20-40 pieces. I have artwork
ready to go. Feel free to forward this note as a request to
prospective service providers.

Appreciate your effort to respond,

Allen
Allen Howells
3430 Broadway
Allentown, PA 18104
cell/ 610.349.5109


#2

Try Ed at LCD in Providence RI;
ldcincorporated.com


#3

Contact Dar Shelton at Sheltech.com. He is the resident Orchid
expert on die cutting.

Joel Schwalb
www.schwalbstudio.com