Aloha, Try SWEST(formerly Southwest Smelting and Refining) the
are as large as Rio and others(and older,1923),11090 North
Stemmons,Dallas,Texas 75229-1389; Phone 214-247-7744(don’t have
the 800 # handy).Have Fun,Nice Town. Regards, Christian Grunewald
Jewelry By Design Precision Modelmaking Hawa ii

Aloha, Try SWEST(formerly Southwest Smelting and Refining) the
are as large as Rio and others

The phone # for Swest is 1-800-527-5057. They also have a web
site: http://www.swestinc.com/index.html (no online catalog,
though, just a few new items listed). This would be a great place
to visit - they are very friendly (on the telephone, anyway) and
have lower prices than Rio Grande. I usually order my silver sheet
and wire from them because they are lower than Hoover and Strong.

Jill
@jandr
http://members.tripod.com/~jilk