I cracked my high school class ring (NMMI, 1983) during a resizing
attempt. I was pretty sure I annealed the 10KW Artcarved ring
adequately, when I went to smite it.
I want to turn it in for value, along with a 14KY cast band, and
gene-splice one ring that reflects both university (Northern Arizona
University, 1988) and high-school. A CAD/CAM approach would be very
interesting.
Contact me off-list. danwoodard36@earthlink.net