Bronze is a higher temp melt than 18K gold. It may be taking too
long to melt. Use the largest tip you can. Bronze also forms a lot
slag, which must be skimmed off. Thirdly, I use a sprinkle of
silicon bronze degasser and stir it in before pouring.
Hope this helps -