i was reading a tip a couple of nights ago about creating your own
stone shape templets for rounds and fancies for wax carving. but i
cant find it, does anyone remember it and could you email it to me.

Thank you
Matthew
email @matthew_gross

i was reading a tip a couple of nights ago about creating your own
stone shape templets for rounds and fancies for wax carving.  but
i cant find it, does anyone remember it and could you email it to
me. 

Hi Matthew,

Is this what you are looking for?

All the best. ekrem.

https://orchid.ganoksin.com/t/source-emerald-cut-deep-basket-wanted
Re: [Orchid] [Source] Emerald cut, deep basket wanted

Hi Sheridan in Chicago!

  Why don't you fabricate your own basket? I learned to take my
  stone (that had a deep belly) imbed it in clay or children's
  play doh, with a  little extra depth to allow for prongs. Then
  pull the stone out gently, fill the cavity with investment and
  let it get hard. When the  investment is hard (an hour or so),
  you pull the investment out of the  clay and turn it over. You
  now have a cast of your stone to create your  basket. Cut your
  wires and solder! Piece of cake! 

  Vi Jones in the beautiful Pacific Northwest