It’s an alloy from Hoover and Strong . It is nice because you
can make 14k green that looks alot like 18k.If you are having
cracking problems then refer back to the post from brainnet on
wed dec 3rd.I have been anealing wrong and letting to much oxy
get to my gold. I also alloy and cast in one step and that’s not
good either.Silver can be used to alloy for a green look but I
don’t know if that is a good thing to do.