Back to Ganoksin | FAQ | Contact

Coloring Quartz

A couple days ago I published a link to an inquiry about coloring
Agates with dyes and acid impregnation. But I forgot to toot my own
horn with a treatise I wrote more descriptive of the irradiation
possibilities. My paper, with photos, contains my own discoveries and
developments you won’t published anywhere except today on the good
Ganoksin list to include the Green Quartz (Ouro Verde) and a method to
make Strawberry Red Quartz.Please comments appreciated.

http://www.liccini.com/Treating/Quartz/Quartz.htm

Mark Liccini

http://www.LICCINI.com