Closing and opening gold-plated jump ring

Risk breaking the gold plating or replace with gold filled and you
can not solder. 

Sorry, posted too late at night, “Breaking”, cracking the gold
plating, you can solder gold filled, not gold plated.

Richard Hart G.G.
Denver, Co.